Re: Large Pit Question
I understand what you are saying, I just haven't experienced it.
Are you using Delta Kits pit resin? If not, what is the viscosity?
It sounds like maybe the problem could be solved by going to a higher viscosity. Our Premium Plate Glass resin is a much higher viscosity and should not seem into the tiny air spaces in the smashed glass. That way you inject your MagniBond, or whatever low viscosity resin you use into the break, enabling you to utilize your pressure and vacuum cycles to remove those tiny air bubbles.
I know some people like to drill out all of the smashed glass, but in most cases my experience has been that the end result is better when it is left in tact.
__________________
Brent Deines
Delta Kits, Inc.
|