Old Blue 66 wrote:Exactly why Im posting about this. Ive noticed a change in how the 4.1 reacts when applied in this heat. Its in the steady 90's now and while Im sure the 4.1 will stil do its thing, I need to change my method of application.
When there are runs or the 4.1 is white right after you apply, will that clear up?
Have you talked to anyone at Delta Kits about adding a bit of water to the coating when mixing? Should slow down the dry time.
ray6
I am used to use shine free paper cups but at the present use HDPE cups with graduations to assist with addition 2k coatings. Fling away what time done. We also utilize throwaway pipettes to move coating from bottle to cup.